BlogStainless Steel castings at high temperature and abrasion in a cemente clinker cooler

In March 2016 Kera-Coat placed 2 cooling plates cast in Mat CrNi 25/12 in a fluidized bed Clinker cooler in the upper and hottest area. In this area The Clinker fells from the kiln as a LAVA river at 1400ºC = 2550ºF while cool air is blown underneath.

Plates are arranged in a way that a moving row pushes the Clinker ahead/downwards over a fixed row. The plates were placed in a fixed row thus suffering the bigger abrasion rate.

We did Not know at that moment which was the average Steel temperature on the plate.